配方类型: SUSPENSIONS AND EMULSIONS
配方说明: Kaolin with Pectin Suspension
配方组成: Distilled Water q.s./100 ml
Pectin/1.0 g
Propyl-p-hydroxy Benzoate/0.08 g
Glycerin/2.0 ml
CMV 7MF/0.075 g
Kaolin 20.0 g
"Avicel" RC-591/0.75 g
Methyl-p-hydroxy Benzoate/0.12 g
配制方法: Disperse the "Avicel" RC-591 and preservatives in 75 ml of distilled water for at least 30 min. Add the CMC 7 MF and mix until completely dispersed. Heat the RC-591-CMC dispersion to 75C and slowly add the pectin and mix until dissolved. Cool the above dispersion and add the glycerin while mixing. Disperse the kaolin until homogeneous being careful to avoid excess air entrapment. Adjust to volume; mix.
Homogenize and/or deaerate if necessary.