返回 化工助手
化学配方数据库
配方类型: ADHESIVES
配方说明: Corrugating Starch (Upper Mixer)
配方组成:
配制方法: Add cold water to 23.75 in. from top. Heat to 130F. and add 180 lb.
corrugating starch. Mix 10 minutes, then add 34 lb. caustic soda in 4 gal. water and mix 15 minutes. Cook with live steam to 165F. and then add water to 6 in. from top.