配方说明: Tin Plating
配方组成: Limiting* value at 70F/250 amp/sq ft
Limiting* value at 100F/425 amp/sq ft
The fluoboric acid is added to 30 gal of water and then the stannous
fluoborate is added. The gelatin is added to 2.7 gal of warm water in a
suitable vessel such as a pail and allowed to swell overnight. The
powdered beta naphthol is added and the mixture stirred continuously
while bringing the mixture to a boil. should the beta naphtol be in
flake form, it should be dissolved in the minimum amount
配制方法: Anodes Pure cast tin is used. They may be bagged with Vinylon, Dynel, or similar materials.
Anode to cathode ratio-from 1:1 to 2:1