化学配方数据库
| 配方类型: | METALS |
| 配方说明: | Rhodium Plating |
| 配方组成: | Sulphuric acid, C.P./100 ml For 0.0003 in. + Plat Replenishment, 5 g/per 4.5 amp.-hr Replenishment, 5 g/per 5 amp.-hr Distilled water/to make 1 gal Rhodium sulphate TP/20 g Rhodium sulphate TP/40 g Sulphuric acid, C.P./100 ml Current density/10-50 ASF Distilled water/to make 1 gal Current density/10-40 ASF |
| 配制方法: | Tank: Glass, plastic-lined steel ("Koroseal"), rigid PVC such as "Boltaron" and "Lucite". Anodes: Platinum or Platanodes (0.04-in. platinum-plated titanium sheet). Anode to cathode ratio, 1/2 to 1 minimum, preferably 1 to 1. Leach all plastic tanks and especially cemented lucite joints, with warm (130F) 10% by volume sulfuric acid for 24 hr. Rinse well. Fill the clean tank half full with distilled or deionized water. Add the required amount of reagent-grade sulfuric acid slowly, with agitation. Mix well. Add the rhodium sulfate TP with stirring. Mix well. Add distilled water to bring liquid level to operating volume. Mix well. Operating Data Temperature Agitation Concentration Current Density |
| 返回数据库查询 |