配方类型: METALS AND THEIR TREATMENT
配方说明: Metal Cleaning Prior to Powder Coating
配方组成:
配制方法: Prior to powder coating the parts pass through a three stage spray washer and phosphatizing machine. Soil is removed in the first stage with a 1-min phosphoric acid spray at 150F, followed by an ambient temperature water rinse for 1/2 min, then a chromic acid rinse at 160F for 1/2 min. Moisture is removed in a 4-min. pass through a dry-off oven at 350F. Cooling time is 8 to 10 min.