化学配方数据库
| 配方类型: | MISCELLANEOUS |
| 配方说明: | Cationic Emulsions of Paraffin Wax |
| 配方组成: | The following formulation requires the use of a colloid mill to produce stable emulsion Water/67.9 ARMAK 1714 Paraffin wax/30.00 ARMAK 1574/0.2 Acetic acid/0.4 ARMAK 1959/1.5 |
| 配制方法: | The Armak chemicals and paraffin are heated until clear, 140F. The melt is added in a thin stream to the water-acetic acid mixture also heated to 140F using good agitation. |
| 返回数据库查询 |