化学配方数据库
| 配方类型: | COATINGS |
| 配方说明: | Metal Coating |
| 配方组成: | Water/250 Letdown "Carboset" 514H Resin/1200 Water/300 Titanium Dioxide/500 Titanium Dioxide/600 "Carboset" 514H Resin (40%)/800 "Carboset" 514H Resin (40%)/1000 Water/300 D.E.R. 332 Epoxy Resin/164 EH 330/24.6 "Carboset" 514H Resin (40%)/500 D.E.R. 332 EH 330 Water/250 "Cymel" 301 Standard Toluene Sulfonic Acid (94%)/115 (15% in ammonia water)/7.5 |
| 配制方法: | This system has 24-48 hr pot life. Bake schedules both systems from 15 min at 350F to 2 min at 400F. |