| 配方说明: | High Wet-Strength Paper Sizing (U.S. Patent 2,549,177) |
| 配方组成: | Oxidized or Chlorinated Starch/1200 Heat for 10 minutes at 80 to 85F. and add Glyoxal/24-60 Water/4800 |
| 配制方法: | Heat for 5 minutes, dilute to 12 liters with water, and cool. Apply at 110 to 150F. |