| 配方类型: | COATINGS |
| 配方说明: | Water-Reducible Alkyd Baking Finish |
| 配方组成: | Ammonium Hydroxide (28%)/31.2 Step 5: Premix following first two components Titanium Dioxide, R-900/307.20 Soln. made in Step 1/140.27 "Resimene" 745/61.44 Water/243.1 Soln. made in Step 1/140.27 "Chempol" 10-0500/564.0 Soln. made in Step 1/409.60/450.60 "FC"-430 (10% in water)/41.00/450.60 2-Ethylhexanol/10.24 "Byk"-H36/1.02 |
| 配制方法: | Mix well. Add ingredients in order listed. Reduce to spray viscosity with 3 parts water for 5 parts enamel (by volume). Flash for 5-10 min and bake 15 min at 350F. |