- 产品名称
- 还原铁粉
- CAS NO
- 7439-89-6
- 中文别名
- 还原铁;还原铁粉状;铁颗粒;铁; 铁精粉; 还原铁,海绵状铁;纳米铁
- 英文名称
- Iron, elemental
- 英文别名
- 300A; 3ZhP;A 131; A 227; A 227 (iron); AC 325; AQ 80; ASC 300; ASC 300 (metal); ATW 230;ATW 432; Ancor B; Ancor EN 80/150; Ancor Image 100; Armco 80; Armco iron; Atomel300M200; Atomel 500M; Atomet 28; Atomet 67; Atomet 95; Atomet 95G; Atomet 95SP;Atomiron 44MR; Atomiron 5M; Atomiron AFP 25; Atomiron AFP 5; BASF-EW; CM; CM(iron); Carbon 0.17, iron 99.83 (atomic); Carbonyl iron; Carbonyl iron powderHQ; Carbonyl iron powder SM; Carbonyl iron powder SU; Copy Powder CS 105-175;DH; DKP; DKP (metal); DM 96; DM 96 (iron); DNK 2R; DSP 1000; DSP 128B; DSP 135;DSP 135C; DSP 138; DT 50 (metal); EF 1000; EF 1000 (metal); EF 250; EFV; EFV200/300; EFV 250; EFV 250/400; EO 5A; EQ; ES; ES (iron); EW 1; Electrolyticiron; F 60; F 60 (metal); FEE; FEE 13PB; FT 3; FT 3 (element); FTF 4; Ferricon;Ferronyl; Ferrovac E; GS 6; H 200; HF 2; HF 2 (element); HL; HL (iron); HQ; HQ(metal); HS; HS (iron); HS 4849; Hoeganaes ATW 230; Hoeganaes EH; ISP 3700;ISP-CIP-R 1470; ISP-S 3700; Iron element; KG 200; KIP 240M; K
- 分子式
-
Fe
- 分子量
- 55.85
- EINECS
- 231-096-4
- 熔点
- 1535°C(lit.)
- 沸点
- 2750°C(lit.)
- 毒性
铁氧体预烧料磁粉。磁性能从3800到4500高斯。粒度从5微米到1微米。
适合做磁材,注塑,尼龙磁粒。
参考信息:cas: 7439-89-6
矫 顽 力:286.62 KA/m
剩 磁:390 T
内禀矫顽力:314.5 KA/m
磁能积:29.2 KJ/m3
材 料 牌号:Y33
密 度:4.2 g/cm3
工 作 温度:250 ℃
居 里 温度:650 ℃
矩 形 比:4000
磁感应强度:12
初始磁导率:3000
铁氧体预烧料粉 是以碳suan锶或碳SUAN贝和氧化铁按照一定比例混合均匀,通过陶瓷工艺(预烧、破碎、制粉、压制成型、烧结和磨加工)制造而成,具有宽磁滞回线、高矫顽力,高剩磁,一经磁化即能保持恒定磁性的功能性材料。铁氧体永磁按工艺可分为两类:其一为烧结永磁铁氧体,其二为粘结永磁铁氧体,烧结永磁铁氧体又分为干压成型与湿压成型,粘结永磁铁氧体分为挤出型、注射型与压延成型。以上各种工艺均可用我司的磁粉作为原料生产